Business

Company endeavoring to satisfy customers with
the continuous technology development and facility investment

thermal spray

Plasma Spray Coating Sample 1 - thermal spray coating Plasma Spray Coating Sample 2 - Korea plasma spray Plasma Spray Coating Sample 3 - plasma coating Plasma Spray Coating Sample 4 - thermal spray coating Plasma Spray Coating Sample 5 - Korea plasma spray Plasma Spray Coating Sample 6 - plasma coating

Plasma Spray Coating

This is the coating method to form the film by injecting the film material to the plasma flow (Speed mach 2 and central temperature: 16,500℃) that is generated from the inert gas by the non-transfer arc and fused momentarily to inject the completely fused powder thermal spray materials in high speed to form the films. For the thermal spray materials, there are broad selection of metals, non-metals, ceramics(mainly the oxide and carbide), and cement, and may have the outstanding films with anti-abrasion, thermal resistance, corrosion resistance, electronic conductivity, electric cover and others, and the repairing is possible with the surface temperature of the processing for thermal spray is controlled within 150℃ that the coating is available for all materials.

coating image

Plasma Spray Coating 1 - thermal spray coating Plasma Spray Coating 2 - Korea plasma spray Plasma Spray Coating 3- thermal spray coating Plasma Spray Coating 4- plasma coating

plasma spray

Material No Ingredients (%) Characteristics Example of application
101 Al2O3- 2%TiO2 - 0.5% SiO2 Gray white color, temperature is outstanding under the high temperature of 550'C for wear resistance, corrosion resistance, acid resistance and others. Textile machine parts, Pump seal
AT35 Al2O3 99% White color, and temperature is outstanding under the high temperature of 800'c or less for wear resistance, corrosion resistance, acid resistance and others with the electric cover Electric insulation part, Textile machine parts, High frequency coil, Semiconductor parts
130 Al2O3 - 13%TiO2 Dark blue with finite tissue, outstanding wear resistance, corrosion resistance, and acid resistance Rewesher, Capstan, Turblne nozzle plug gaude, Textile machine parts
131 Al2O3 - 40%TiO2 Dark. blue, temperature of 550'C or below, electric conductivity Textile machine parts, Machine parts
106 Cr2O3 - 2%TiO2 dark brown, high degree of hardness, workable temperature below than 540℃, excellent wear resistance, acid resistance and alkaline resistance, The texture is dense. mechanical seal, parts of textile machinery, wearing, roll
ZT25, ZT75, ZT60 ZrO2 - 8%Y2O3 rust proofing of particles at the 1000℃ of workable temperature, thermal resistance, prevention of oxidation nozzle of rocket, missile cap, tray for high temperature
YT15, YT25, YT35 Y2O3 1500℃ of workable temperature, plasma resistance, prevention of oxidation OLED, SEMI Part’s, tray for high temperature